一.Product Description
1. The anodizing production line necessitates meticulous control of
equipment and stringent regulation of process parameters, including
current density, temperature, time, and more. Mastery of these
critical process variables is essential for the creation of
high-quality anodized products.
2. Anodizing finds extensive application in the surface treatment
of components across various industries such as aerospace,
automotive, and electronics. It not only enhances product
performance but also elevates its aesthetic appeal.
3. With the relentless advancement of technology, anodizing
techniques are continually being optimized and upgraded to offer
superior surface treatment solutions tailored for diverse
industries.
二. Design Condition
1 | Alloy | Aluminium 6061 to 6063 or others |
2 | Anodizing film thinkness | 10~ 12µm m |
3 | Average coverage area | 350m²/T (ton) |
4 | Max aluminium profile length | 6500mm |
5 | Extrusion ratio | 2.5kg/m² |
6 | Working hour/m | 300d/m x 20h/d = 600h/m |
7 | Racking system | Two fixtures /rack |
8 | Racking operation | Manual |
9 | Equipment Usage Rate | 0.9 |
10 | Power supply | AC 3phase 380v 50hz |
11 | Control Power | AC220V 50Hz |
12 | Water supply | 2kg/cm²·G |
13 | Hot steam | 6kg/cm²·G |
14 | Compressor air | 6kg/cm²·G |
三.Process Tank
1 | Degreasing 【Free sulfuric acid 180±30 g/l】 | 1 Tank |
2 | Alkaline Etching【Free alkali 40-60g/l,Al3+ 30-120g/】 | 2 Tanks |
3 | Neutralization 【Free sulfuric acid180±20g/l】 | 1 Tank |
4 | Anodising 【Free sulfuric acid 140-180g/l,Al3+≤20g/l】 | 4 Tanks |
5 | Colouring 【stannous sulfate 3-8g/l,Free sulfuric acid 15-25g/l,PH 0.8-1.2】 | 2 Tanks |
6 | Medium Temperature Sealing【PH 5-6.5,Nickel ion0.8-1.3g/l,Fluorion0.3-0.7 g/l】 | 3 Tank |
四.Treatment Process:
(6) Average anodizing layer : 0.3*1.3*30*0.77 =10.81um
1) Clour process: Mix Salts
2) Quantity:2 jig(rack)/tank x 1tanks = 2jig(rack)
3) Current density: 70A
4) Process time: 2-8min
6. Sealing
1) Sealing menthod: Sealing at Medium or Normal Temperature
2) Quantity:6jig(rack)/tank x 1 tank
3) Process time 10-15min
五. Design Parameter and Setting
1. Anodizing treatment area:
1) Each anodizing process tank need 40min ,where total
jig(rack)/year:
( 2 rack x 4 tank x 60min/h) ÷40min x600 hour =7200jig(rack)
2) Design 50m²/jig(rack) . Where every tank is 100m²
3) Area treatment/year : 7200jig(rack)x 50m² /jig =360000m²
2. Anodizing treatment weight:
Monthly output :
360000m²÷350m²/T*0.6=617T≧600T
3. Power consumption:
1) Anodising Tank:100m²/tank* 130A/ m²÷0.2=A/tank
Power Rectifier : 15000A =4unit
2) Clouring tank: 100㎡/tank×70A/m²÷0.9 = 7777A/tank
Colour Rectifier : 8000A =2unit
六. Process Chat
Discription for Un | ||
1 | De | Degreasing |
2 | Rs | Rinsing |
3 | HW Rs | Hot Water Rinsing |
4 | AE | Alkaline Etching |
5 | Ne | Neutralization |
6 | An | Anodizing |
7 | Cl | Coloring |
8 | Sl | Sealing |
9 | MU | Material Unloading |
10 | Pc | Packing |
catalogue uploading :
PDF Gallery_20240719_102320.pdf01_0.pdf04.pdf07.pdf10_0.pdf12.pdf15_0.pdf18.pdf
Transportation&Packaging
![]() |